GJB3317 GH163 GH4163 AMS5872 Haynes 263 Nimonic 263 N07263 Nickel Alloy Sheet
Shape |
Round,Forging,Ring,Coil,Flange,Disc,Foil,Spherical,Ribbon,Square,Bar,Pipe,Sheet |
Grade |
Duplex: 2205(UNS S31803/S32205),2507(UNS S32750),UNS S32760(Zeron 100),2304,904L |
|
Others:253Ma,254SMo,654SMo,F50(UNSS32100)F60,F61,F65,1J22,N4,N6 etc |
|
Alloy : Alloy 20/28/31 |
|
Hastelloy:HastelloyB/ -2/B-3/C22/C-4/S/ C276/C-2000/G-35/G-30/X/N/g |
|
Hastelloy B / UNS N10001,Hastelloy B-2 / UNS N10665 / DIN W. Nr. 2.4617,Hastelloy C, Hastelloy C-4 / UNS N06455 / DIN W. Nr. 2.4610,Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602, Hastelloy C-276 / UNS N10276 / DIN W. Nr. 2.4819,Hastelloy X / UNS N06002 / DIN W. Nr. 2.4665 |
|
Haynes: Haynes 230/556/188/263 |
|
Inconel 600/601/602CA/617/625/713/718/738/X-750,Carpenter 20 |
|
Inconel 718 / UNS N07718 / DIN W. Nr. 2.4668,Inconel 601 / UNS N06601 / DIN W. Nr. 2.4851, Inconel 625 / UNS N06625 / DIN W. Nr. 2.4856,Inconel 725 / UNS N07725,Inconel X-750 / UNS N07750 / DIN W. Nr. 2.4669,Inconel 600 / UNS N06600 / DIN W. Nr. 2.4816 |
|
Incoloy: Incoloy 800/800H/800HT/825/925/926; |
|
GH: GH2132,GH3030,GH3039,GH3128,GH4180,GH3044 |
|
Monel: Monel 400/K500/R405 |
|
Nitronic: Nitronic 40/50/60; |
|
Nimonic: Nimonic 75/80A/90/A263 ; |
Specification |
Wire: 0.01-10mm |
Haynes 263 is an age-hardenable nickel-cobalt-chromium-molybdenum alloy designed specifically to combine very good strength properties with excellent fabrication characteristics in the annealed condition. While its strength at elevated temperatures is not quite as high as materials such as Waspaloy or alloy R-41, it is far easier to form or weld than these alloys. Alloy 263 exhibits excellent intermediate temperature tensile ductility, and is not normally subject to strain age cracking problems common for gamma prime strengthened alloys.
Nickel: Balance
Cobalt: 19.00 - 21.00
Chromium: 19.00 - 21.00
Molybdenum: 5.60 - 6.10
Titanium: 1.9-2.4
Titanium + Carbon: 0.04-0.08
Aluminum: .0.60 max
Manganese: 0.60 max
Silicon: 0.40 max
Iron: 0.70 max
Boron: 0.005 max
Copper: 0.20 max
Sulfur: 0.007 max
Silver: 0.0005 max
Bismuth: 0.0001 max
Density: 0.302 lbs/in3, 8.36 g/cm3
Electrical Resistivity: micro-ohm-in, (micro-ohm-cm):
70 °F (21 °C): 45.3 (115)
Mean Coefficient of Thermal Expansion: µin/in-°F (µm/m-°C)
70 - 200 °F (25 - 100 °C): 6.2 (11.1)
70 - 400 °F (25 - 200 °C): 6.7 (12.1)
70 - 600 °F (25 - 300 °C): 7.1 (12.7)
70 - 800 °F (25 - 400 °C): 7.2 (12.8)
70 - 1000 °F (25 - 500 °C): 7.6 (13.6)
70 - 1200 °F (25 - 600 °C): 7.9 (13.9)
70 - 1400 °F (25 - 700 °C): 8.3 (14.7)
70 - 1600 °F (25 - 800 °C): 9.0 (15.4)
70 - 1800 °F (25 - 900 °C): 9.9 (17.0)
Thermal Conductivity: BTU-in/ft-°F (W/m-°K)
70 °F (21 °C): 81 (11.7)
200 °F (100 °C): 89 (13.0)
400 °F (200 °C): 103 (14.7)
600 °F (300 °C): 115 (16.3)
800 °F (400 °C): 128 (18.0)
1000 °F (500 °C): 141 (19.7)
1200 °F (600 °C): 154 (21.2)
1400 °F (700 °C): 167 (23.0)
1600 °F (800 °C): 182 (24.7)
1800 °F (900 °C): 195 (26.8)
Modulus of Elasticity: KSI (MPa)
32.1 x 103 (221 x 103) in tension
Melting Range: 2370 - 2470 °F (1300 - 1355 °C)
Coil - Strip, Foil, Ribbon Wire - Profile, Round, Flat, Square
The following table shows mechanical properties of HAYNES 263 (solution-treated and aged).
Properties | Metric | Imperial |
---|---|---|
Tensile strength | 1050 MPa | 152.3 ksi |
Yield strength | 635 MPa | 91.9 ksi |
Elastic modulus | 221 GPa | 32.1 psi |
Elongation at break | 35.70% | 35.70% |
The thermal properties of HAYNES 263 are tabulated below.
Properties | Metric | Imperial |
---|---|---|
Thermal expansion co-efficient (@25-200°C/77-392°F) | 11 .1 µm/m°C | 6.2 µin/in°F |
Thermal conductivity | 11.7 W/mK | 81 BTU in/hr.ft².°F |
HAYNES 263 is used in the following application areas: