| Customization: | Available |
|---|---|
| Application: | Aviation, Electronics, Industrial, Medical, Chemical |
| Standard: | JIS, GB, DIN, ASTM, AISI |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency


Rectangle Polished Inconel 625 Nickel Based Alloy Pipe for Jet engine
Inconel 625 is a nickel-based super alloy that possesses excellent resistance to oxidation and corrosion in a broad range of environments. Additionally this alloy has outstanding strength and toughness at temperatures ranging from cryogenic to 2000°F. This alloy possesses a high degree of formability and shows better weldability than many other highly alloyed nickel based materials.
Typical chemical analysis of Inconel 625.
| Element | Percentage |
| Carbon | 0.010 max |
| Manganese | 0.50 max |
| Phosphorus | 0.015 max |
| Sulfur | 0.015 max |
| Silicon | 0.50 max |
| Chromium | 20.00 - 23.00 |
| Nickel | Balance |
| Molybdenum | 8.00 - 10.00 |
| Iron | 5.00 max |
| Titanium | 0.40 max |
| Aluminum | 0.40 max |
| Tantalum | 0.05 max |
Thermal conductivity data as a function of temperature for Inconel 625 is provided in the follwoing table.
| Temperature Range |
Linear Coefficients of Thermal Expansion1 |
Thermal Conductivity2 3 | ||||||||||
| °C | °F | /°C | /°F | W/m·K | Btu/(hr/ft²/in/°F) | |||||||
| -157 | -250 | - | - | 7.3 | 4.2 | |||||||
| -129 | -200 | - | - | 7.4 | 4.3 | |||||||
| -73 | -100 | - | - | 8.3 | 4.8 | |||||||
| -18 | 0 | - | - | 9.2 | 5.3 | |||||||
| 21 | 70 | - | - | 9.9 | 5.7 | |||||||
| 38 | 100 | - | - | 10.0 | 5.8 | |||||||
| 93 | 200 | 12.8 | 7.1 | 10.7 | 6.3 | |||||||
| 204 | 400 | 13.1 | 7.3 | 12.6 | 7.3 | |||||||
| 316 | 600 | 13.3 | 7.4 | 14.2 | 8.2 | |||||||
| 427 | 800 | 13.7 | 7.6 | 15.7 | 9.1 | |||||||
| 538 | 1000 | 14.0 | 7.8 | 17.5 | 10.1 | |||||||
| 649 | 1200 | 14.8 | 8.2 | 19.0 | 11.0 | |||||||
| 760 | 1400 | 15.3 | 8.5 | 20.8 | 12.0 | |||||||
| 871 | 1600 | 15.8 | 8.8 | 22.8 | 13.2 | |||||||
| 927 | 1700 | 16.2 | 9.0 | - | - | |||||||
| 982 | 1800 | - | - | 25.3 | 14.6 | |||||||
Typical room temperature tensile properties of Inconel 625 annealed at 1920°F (1065°C) follow.
| Temperature | 0.2% Yield Strength | Ultimate Tensile Strength | Elongation Percent | |||
| °F | °C | psi | MPa | psi | MPa | |
| 1920 | 1065 | 63,000 | 430 | 136,000 | 940 | 51.5 |
United Performance Metals Inconel 625 is supplied to AMS 5599 and UNS Designation N06625.
Inconel 625 is typically used for: